Colour masterbatches are very simple to use: they simply need to be thoroughly mixed with plastic resin in the correct proportions, adapted to the requirements of various plastic processing methods, and then extruded.
It is important to note that when changing colours, the hopper must be thoroughly cleaned; any residual material in the machine’s barrel must be flushed out using plain plastic or a screw cleaner, and a new filter screen with a mesh size of 100 mesh or higher must be fitted. Ensure that the temperature is set correctly to prevent any colour changes.
Common problems encountered when colouring plastic products and how to resolve them:
1. Grain formation on the product surface:
Main reasons:
① There are impurities in the barrel and die head;
② The temperature is incorrect;
③ The raw materials remain in the barrel for too long whilst being heated;
④ The dispersion of the colour masterbatch or colour powder has not been properly managed;
⑤ The filter mesh is perforated.
Procedure:
Adjust the temperature of the extruder to 10–20 °C below the normal setting, start the extruder, and run a cleaning cycle at low speed using uncoloured plastic resin. If necessary, dismantle the die head for cleaning, adjust the temperature accordingly, and replace the filter screen promptly. Switch to a well-dispersed colour masterbatch or colour powder and carry out the commissioning process again.
2. Uneven diffusion:
Main reasons:
① Incomplete mixing;
② Inappropriate temperature;
③ Poor compatibility between the colour masterbatch and the raw material;
④ The plasticising performance of the injection moulding machine itself is poor;
⑤ The proportion of colour masterbatch used is too low.
Remedial measures: Stir thoroughly, adjust the temperature to the correct level, replace the colour masterbatch or raw materials, switch to another production line, or adjust the proportion of colour masterbatch added.
3. Frequent material shortages:
Main reasons:
① The temperature is incorrect;
② Poor affinity for the substrate;
③ Poor dispersion of the colour masterbatch;
④ The proportion of colour masterbatch used is too high.
Solution: Adjust the temperature accurately, change the raw materials used, switch to a colour masterbatch with good dispersion properties, and reduce the proportion of colour masterbatch used.
4. Colour changes:
Main reasons:
① The base colours of the raw materials used are inconsistent;
② The plastic moulding machine has not been cleaned thoroughly;
③ The colour masterbatch or colour powder used has a low temperature resistance and loses its colour when the temperature is too high;
④ The feed door has not been cleaned properly;
⑤ Changes to the manufacturing process;
⑥ Colour masterbatches or colour powders exhibit colour variations;
⑦ Inappropriate gate material selection;
⑧ The mixer has not been cleaned thoroughly or the mixing time has not been controlled properly.
Solution: Use raw materials that match the colour of the test sample and adjust the ratio of scrap material accordingly; thoroughly clean the injection moulding machine, the feed gate and the mixer; switch to a colour masterbatch or colour powder with suitable heat resistance and a consistent colour; and employ a stable processing method.
As there are many factors that can influence the production process, we recommend that users carry out their own trial runs with the Red Plum masterbatch to achieve the desired results. Should you encounter any issues during the trial runs that you are unable to resolve, please do not hesitate to contact us; we will do our utmost to assist you in resolving every issue.